Cracks or fractures formed in a casting prior to completion of solidification because of restricted contracting are indicative of a
a. Shrinkage defect
b. Porosity defect
c. Cold shut defect
d. Hot tear defect

Respuesta :

Otras preguntas

Geometry math question no Guessing and Please show work
If square LMNO is dilated by a scale factor of two about the center of the square to create square L'M'N'O', dilated line P'Q' will (5 points) Question 6 optio
What times what is y to the 6th?
Anybody know the answer?
Write an equation in a slope-intercept form for the line described. 1. Slope -2, passes through (-4,6) 2. Slope 1, passes through (2,5)
how many different ways can you make words using the letters A.B E & L
Solve equation 10(-2q - 16) = 40
With respect to leadership in the accounting profession, it might be said that: rev: 04_19_2017_qc_cs-86230  partners must exhibit moral imagination through et
prime # between 17 and 23 and its double
A square piece of paper is folded in half vertically. the resulting figure has a perimeter of 21 inches. What is the number of square inches in the area of the